Abstrait

Synthesis and characterization of new polyamides bearing á,á-xylyldithiophenoxide units in the main chain: Microwave irradiation, nanostructures

Esmael Rostami, Abdolkarim Zare, Masume Zangooei


Newpolyamides containing á,áï‚¢-Xylyldithiophenoxide Unitswere prepared under microwave irradiation and their solubility, thermal behavior, viscosities and nanostructures were evaluated. These polyamides showed good solubility in a series of organic solvents. The viscosities of these polyamides are in the range of 0.41-0.54 dl/g. Glass transition temperatures are in the range of 214-251°C. Temperatures for 10% weight loss (T10) are in the range of 286-323°C, temperatures for 50% weight loss (T50) are in the range of 463-535°C and char yields are in the range of 21-41%; and these results shows the thermal stabilities of the prepared polyamides. Supramolecular assemblies showed nanostructures.


Avertissement: testCe résumé a été traduit à l'aide d'outils d'intelligence artificielle et n'a pas encore été examiné ni vérifié

Indexé dans

  • CASS
  • Google Scholar
  • Ouvrir la porte J
  • Infrastructure nationale du savoir de Chine (CNKI)
  • CiterFactor
  • Cosmos SI
  • Répertoire d’indexation des revues de recherche (DRJI)
  • Laboratoires secrets des moteurs de recherche
  • Facteur d’impact des articles scientifiques (SAJI))
  • ICMJE

Voir plus

Flyer